MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

(Viewing data as-entered. Click here to return)
Aremco Aremcolox™ 502-1820 Boron Nitride - Aluminum Nitride Composite
Categories: Ceramic; Ceramic Matrix Composite; Nitride

Material Notes: Hot-pressed BN-AlN demonstrates high thermal conductivity and electrical resistivity, and good mechanical properties compared to BN. For use at temperatures to 1000 ºC in air and 1800 ºC in a vacuum or inert atmosphere. Ideal for applications requiring high thermal conductivity and electrical insulation in the semiconductor industry.

Key Words: BN + AlN
Vendors: Aremco’s Dense Ceramics — BN Compositesare suitable for applications up to 1830°F (1100°C) in oxidizing environments and 3270°F (1800°C) in inert atmospheres. Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Aremco offers a range of boron nitride composites. Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 2.75 - 2.85 g/cc
Water Absorption 1.3 %
 
Mechanical PropertiesOriginal ValueComments
Flexural Strength 12325 psi
Compressive Strength 27725 psi
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1e+13 ohm-cmDC
Dielectric Constant 7.2
@Frequency 1e+6 Hz
 
Thermal PropertiesOriginal ValueComments
CTE, linear 1.60 µin/in-°F
Thermal Conductivity 85.0 W/m-K
Maximum Service Temperature, Air 1830 °FOxidizing
Maximum Service Temperature, Inert 1800 °CVacuum
 1800 °CInert
 
Descriptive Properties
ColorGrey

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

CAREM981 / 282877

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.