MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Amodel® A-1133 NL WH 505 PPA, 33% glass fiber
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 30% Glass Fiber Reinforced

Material Notes: 33% glass fiber, high-reflectivity white for LEDs

Amodel® A-1133 NL resin is a 33% glass reinforced polyphthalamide (PPA) which is distinguished by its high-reflectivity white color. This grade features a high deflection temperature for compatibility with SMT processes, and low moisture absorption.

- White: A-1133 NL WH 505

Markets/Uses: Automotive / Automotive E/E / LEDs

Applications: Automotive Electronics; Housings; LEDs

Features: Chemical Resistant; Good Color Stability; High Reflectivity; Low Moisture Absorption

Injection notes: A general purpose screw is recommended, with minimum back pressure.
Storage:
- Amodel® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Amodel® resins be dried prior to molding following the recommendations found in this datasheet and/or in the Amodel® processing guide.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.54 g/ccMethod A; ISO 1183
Water Absorption 0.16 %
@Time 86400 sec
ASTM D570
Linear Mold Shrinkage, Flow 0.0020 cm/cmASTM D955
Linear Mold Shrinkage, Transverse 0.0060 cm/cmASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 125ASTM D785
Tensile Strength at Break 179 MPaASTM D638
Elongation at Break 1.8 %ASTM D638
Tensile Modulus 12400 MPaASTM D638
Flexural Yield Strength 236 MPaASTM D790
Flexural Modulus 11700 MPaASTM D790
Poissons Ratio 0.41ASTM E132
Izod Impact, Notched 37.0 J/mASTM D256
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 14.0 µm/m-°C
@Temperature 160 - 249 °C
ASTM E831
 23.0 µm/m-°C
@Temperature 0.000 - 100 °C
ASTM E831
CTE, linear, Transverse to Flow 4.50 µm/m-°C
@Temperature 0.000 - 100 °C
ASTM E831
 100 µm/m-°C
@Temperature 160 - 249 °C
ASTM E831
Melting Point 310 °C
Deflection Temperature at 1.8 MPa (264 psi) 271 °CUnannealed; ASTM D648
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 304 - 318 °C
Front Barrel Temperature 316 - 329 °C
Melt Temperature 321 - 343 °CInjection
Mold Temperature 135 °C
Drying Temperature 120 °C
@Time 14400 sec
Moisture Content <= 0.045 %Injection
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorWhite
FormsPellets
ProcessingInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4040 / 279840

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.