MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

(Viewing data as-entered. Click here to return)
Ensinger TECANYL GF30 natural Polyphenylene ether, 30% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyphenylene Ether/PPO; Polyphenylene Ether, 30% Glass Filled

Material Notes:
  • very high stiffness
  • electrically insulating
  • good weldable and bondable
  • sensitive to stress cracking
  • high strength
  • high dimensional stability
Target Industries:
  • electrical engineering
  • precision engineering
  • conveyor technology
  • mechanical engineering
  • power engineering
  • automotive industry
  • home appliances

Information provided by Ensinger Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.30 g/cc
Water Absorption 0.010 %
@Time 86400 sec
DIN EN ISO 62
 0.20 %
@Time 346000 sec
DIN EN ISO 62
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 205 MPaISO 2039-1
Tensile Strength 73.0 MPa50mm/min; DIN EN ISO 527-2
Elongation at Break 5.0 %50mm/min; DIN EN ISO 527-2
Elongation at Yield 5.0 %50mm/min; DIN EN ISO 527-2
Modulus of Elasticity 4.10 GPa1mm/min; DIN EN ISO 527-2
Flexural Strength 116 MPa
@Load 1.02 kg
2mm/min; DIN EN ISO 178
Flexural Modulus 3900 MPa
@Load 1.02 kg
2mm/min; DIN EN ISO 178
Compressive Strength 23.0 MPa
@Strain 1 %,
Load 1.02 kg
5mm/min; EN ISO 604
 41.0 MPa
@Strain 2 %,
Load 1.02 kg
5mm/min; EN ISO 604
Compressive Modulus 3300 MPa
@Load 1.02 kg
5mm/min; EN ISO 604
Charpy Impact Unnotched 37.0 kJ/m²max. 7,5J; DIN EN ISO 179-1eU
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmDIN IEC 60093
Surface Resistance 1.00e+14 ohmDIN IEC 60093
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 40.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
DIN EN ISO 11359-1;2
 40.0 µm/m-°C
@Temperature 23.0 - 100 °C
DIN EN ISO 11359-1;2
Specific Heat Capacity 1.20 J/g-°CISO 22007-4:2008
Thermal Conductivity 0.280 W/m-KISO 22007-4:2008
Maximum Service Temperature, Air 85.0 °Clong term
 110 °Cshort term
Glass Transition Temp, Tg 150 °CDIN 53765
Flammability, UL94 HBDIN IEC 60695-11-10
 
Descriptive Properties
Colorbeige opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PENSIN8175 / 319103

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.