MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Eastman Eastek™ 4500 Polyester
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Eastman Eastek™ 4500 polymer is a high-performance polyester resin for polyurethane hot melt adhesive applications. Eastman Eastek 4500 polymer is designed to reduce viscosity, increase Tg, enhance UV resistance, and improve formulation compatibility to enable greater productivity, application consistency, and long-term durability of the bonded structure.

Applications

  • Adhesives
  • Polyurethanes
Key Attributes
  • Enhanced compatibility with tackifiers
  • Excellent green strength
  • Good heat and hydrolytic stability
  • High Tg
  • Low viscosity
  • Outstanding UV resistance
  • Superior adhesion to low surface energy substrates

Information provided by Eastman.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Brookfield Viscosity 9000 - 12000 cP
@Temperature 130 °C
 
Chemical PropertiesOriginal ValueComments
Total Acid Number <= 1.50[mg KOH/g]; ASTM D664
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg 44.0 - 46.0 °C
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.100 %ASTM D1533
 
Descriptive Properties
Color<200ASTM D1209
Hydroxyl Number38-43 mg KOH/gASTM E222
Open Time<5 sec

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PEATM4132 / 323755

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.