System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Evonik VESTAMID® E62-S1 Nylon 12 Elastomer
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 12 (PA12)
Material Notes:
Heat- and light-stabilized compound based on polyamide 12 elastomer for molding of sport shoe soles.
Property data for dry samples.
Information provided by Evonik.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Mechanical Properties
Metric
English
Comments
Tensile Strength at Break
40.0
MPa
5800
psi
ISO 527
Elongation at Break
278 %
278 %
ISO 527
Tensile Modulus
0.389
GPa
56.4
ksi
ISO 527
50% Modulus
23.0
MPa
@Strain 50 %
23.0
MPa
@Strain 50 %
ISO 527
Charpy Impact, Notched
12.1
J/cm²
@Temperature 23.0 °C
57.6
ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
Thermal Properties
Metric
English
Comments
Melting Point
172
°C
342
°F
ISO 11357-1/-3
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Arkema Pebax® 7033 SA 01 MED Polyether Block Amide (PEBA)
Evonik VESTAMID® E47-S1 Nylon 12 Elastomer
EMS-Grivory Grilamid® L 25 Z PA12-I
Evonik VESTAMID® Care ML21 Medical Grade Nylon 12
Arkema Pebax® 7433 SA 01 MED TPA
PEVONIK831 / 243040
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.