MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Copper Alloy, UNS C81540, TF00 Temper, As Sand Cast
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Precipitation Hardened

Casting Characteristics: High – Drossing, Effect of Section Size; Medium – Fluidity, Gassing, Shrinkage in Solidification; Low - Casting Yield

Fabrication Properties: Good Suitability – Gas Shielded Arc Welding; Fair Suitability – Soldering

Typical uses: Blow Mold Cavities; Blow Pins for Blow Molds; Cavities for Injection Molds; Core Pins for Injection Molds; Cores for Injection Molds; Ejector Pins for Injection Molds; Flash Weld Dies; Hot Runner Systems for Injection Molds; Molds for Plastic Parts; Pinch Offs for Blow Molds; Resistance Welding Gun Arms; Resistance Welding Tips; Resistance Welding Wheels; Sprue Bushings for Injection Molds; Stud Welding Collets; Tip Welding Collets

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.315 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 210
@Load 3000 kg
Tensile Strength 100 ksi
Tensile Strength, Yield 75.0 ksi0.5% Ext
Elongation at Break 13 %
Tensile Modulus 16000 ksi
Modulus of Rigidity 6154 ksiCalculated
Poissons Ratio 0.30
Machinability 40 %
Charpy Impact 25.0 ft-lbV-Notch
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000360 ohm-cm48% IACS
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.70 µin/in-°F
@Temperature 20.0 - 200 °C
Specific Heat Capacity 0.100 BTU/lb-°F
Thermal Conductivity 125 BTU-in/hr-ft²-°F
Melting Point 2021 - 2039 °F
Solidus 2021 °F
Liquidus 2039 °F
Shrinkage 2.08 %Patternmaker's Shrinkage (4/16 in./ft.)
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al <= 0.10 %
Chromium, Cr 0.10 - 0.60 %
Copper, Cu >= 95.1 %
Iron, Fe <= 0.15 %
Lead, Pb <= 0.020 %
Nickel, Ni 2.0 - 3.0 %
Silicon, Si 0.40 - 0.80 %
Tin, Sn <= 0.10 %
Zinc, Zn <= 0.10 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC81540x1 / 292531

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.