MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
KLJ Group KANATOL 9090 Plasticizer
Categories: Fluid

Material Notes: Properties: Kanatol-9090 is transparent liquid with stability and soluble in most of organics solvent. This product is a primary plasticizer with fine performances. Most preferable Plasticizer, to be used in PVC, chlorethlene polymer, cellulose nitrate, ethyl cellulose and synthetic rubber.

Application: Easily dissolved with PVC, as its volatility, migration and non-toxicity are superior to DOP. It can present products with good light resistance, heat resistance, degradation resistance and electrical insulation. Finds applications as Non-Carcinogen plasticizer in toy film, vinyl gloves, wall covering, vinyl flooring, carpet & novelties and synthetic rubber, wires and cables owing to its excellent properties of water fastness, low toxicity, degradation resistance, electrical insulation than DOP. It has lower flexibility cause of its structure, and this decrease plastics fragile of lower heat. Due to its structural behavior, it can lubricate itself and conclusion of this, preparing plastisol is much more shorter time and spending less energy. It can replace DINP, DIDP due to lower volatile character. Preferable plasticizer for producing cable with excellent electrical specialties.

Chemical Name: Di-Iso-nonyl benzene 1, 4, di carboxylate

Molecular Formula: C 26 H42 O 4

Molecular Structure: C6 H4 -1, 4-[CO2 C9 H17 ] 2

Information provided by KLJ Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.962 - 0.968 g/cc
@Temperature 27.0 °C
ASTM D1045-08
Viscosity 80 - 86 cPKLJ TM-P-13-97
Molecular Weight 418 g/mol
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 175 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.483 - 1.489
@Temperature 27.0 °C
ASTM D1045-08
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.10 %ASTM E203-08
Shelf Life 24.0 Month
 
Descriptive Properties
Acidity after heat treatment<0.03%180°C for 2 hrs, ISI-9591-03
Acidity as Acid<0.01%ASTM D1045-08
AppearanceWater White Clear Liquid
Color<20Hazen, ASTM D1045-08
Content>99.5%Ester Content, ASTM D1045-08
 >99.5%Plasticizing Ester by GLC, KLJ TM-P-12-98
 265-271 mg KOH/gmEster Value, ASTM D1045-08
Volatile Loss<0.1%130°C for 3 hrs, KLJ TM-P-11-92

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PKLJ249 / 284270

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.