MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Claude Bamberger Bamberko® 9016 Purge Compound
Categories: Polymer; Thermoplastic; Purging Compound

Material Notes: Bamberko® is recommended for cellulosics, polyolefins, styrenics, and PVC resins. Temperature range 350-525°F (176-275°C). Formulated to flow through injection cylinders and extrusion barrels without scratching. Recommended for use in swift color and resin changeover and to clean machines of carbonized residue. BAMBERKO® will not melt completely and are excellent for difficult purging jobs.

Information provided by Claude Bamberger Molding Compounds.

Key Words: Purging Compound
Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 350 - 450 °FCellulosics, Polyolefins, Styrenics & PVC Resins
 400 - 550 °FHigh Temperature Engineering Plastics

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Abatron AboCoat 8508-1 Heavy-Duty Epoxy Paint
SSAB Tunnplat Docol® DC01 (Fe P01) Deep-drawing Steel
Envalior Durethan® BKV 230 H2.0 901510 Copolyamide, 30% Glass Fiber
EN S355JR High Manganese, Structural, Hot Rolled, Base Steel
EN S355J0 High Manganese, Structural, Hot Rolled, Quality Steel

PCBAM0 / 27947

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.