MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

UBE UPIA® LB Polyimide
Categories: Polymer; Thermoset; Polyimide, TS

Material Notes: UPIA® is a polyimide precursor formed from UBE's proprietary BPDA(Biphenyl tetracarboxylic dianhydride) monomers. This is the original UBE varnish. UBE polyimide film "UPILEX®" is produced using this unique UBE polyimide precursor giving it various and unique advantages. Polyimide coated film derived from the varnish of the same grade has the same properties. UPIA® can be used at any desired concentration by diluting it with anhydrous NMP or DMAc (N, N-dimethylacetamide). UPIA® has superior storage stability compared to conventional polyimide varnishes. It exhibits a very low increase in viscosity at room temperature, while conventional polyimide varnish must be refrigerated or frozen.

Information provided by UBE Industries, LTD

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.05 - 1.15 g/cc0.0379 - 0.0415 lb/in³
Solids Content 10 - 30 %
@Temperature 350 °C,
Time 1800 sec
10 - 30 %
@Temperature 662 °F,
Time 0.500 hour
Viscosity 100 - 10000 cP
@Temperature 30.0 °C
100 - 10000 cP
@Temperature 86.0 °F
E-type Solution Viscosity in NMP

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PUBD9857 / 287320

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.