MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Copper Alloy, UNS C18150, TL04 Temper, Rod
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Precipitation Heat Treated or Spinodal Heat Treated and Hard

Common Fabrication Processes: Bending, Cold Heading, Machining

Typical Uses: Pencil-type & Light Soldering Guns: Tips, Rod Extensions; Resistance welding electrodes; Welding Electrodes; Welding Wheels, Tips and Rod Extensions

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.89 g/cc0.321 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell B  78
@Thickness 19.0 mm
78
@Thickness 0.750 in
 82
@Thickness 12.3 mm
82
@Thickness 0.485 in
Tensile Strength  545 MPa
@Thickness 19.0 mm
79000 psi
@Thickness 0.750 in
 558 MPa
@Thickness 12.3 mm
81000 psi
@Thickness 0.485 in
Tensile Strength, Yield  517 MPa
@Thickness 19.0 mm
75000 psi
@Thickness 0.750 in
0.5% Ext
 545 MPa
@Thickness 12.3 mm
79000 psi
@Thickness 0.485 in
0.5% Ext
Elongation at Break  14 %
@Thickness 12.3 mm
14 %
@Thickness 0.485 in
 16 %
@Thickness 19.0 mm
16 %
@Thickness 0.750 in
Tensile Modulus 117 GPa17000 ksi
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000220 ohm-cm0.00000220 ohm-cm80% IACS
 
Thermal PropertiesMetricEnglishComments
CTE, linear 17.1 µm/m-°C
@Temperature 20.0 - 100 °C
9.50 µin/in-°F
@Temperature 68.0 - 212 °F
Thermal Conductivity 26.9 W/m-K187 BTU-in/hr-ft²-°F
Melting Point 1070 - 1080 °C1958 - 1976 °F
Solidus 1070 °C1958 °F
Liquidus 1080 °C1976 °F
Annealing Point 982 - 1010 °C1800 - 1850 °F
 
Processing PropertiesMetricEnglishComments
Hot-Working Temperature 816 - 927 °C1500 - 1700 °F
Precipitation Temperature >= 427 °C>= 800 °F
 
Component Elements PropertiesMetricEnglishComments
Chromium, Cr 0.50 - 1.5 %0.50 - 1.5 %
Copper, Cu 98.3 - 99.5 %98.3 - 99.5 %As Balance
Zirconium, Zr 0.020 - 0.20 %0.020 - 0.20 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC18150x1 / 291644

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.