MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Persian Gulf Polymer GPPS-0503 General Purpose Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Molded, Unreinforced

Material Notes: General purpose polystyrene (GPPS) 0503 is a high molecular weight crystal polystyrene which allows maximum dilution rates with high impact polystyrene grades. In dilution, polystyrene crystal 0503 gives excellent processing in both extrusion and thermoforming with good finished product dimensional stability. Application: It is recommended for cups and other products by in line extrusion thermoforming, foamed trays by direct gassing, dairy sheets, CD boxes, toys, and office equipment.

Information provided by Persian Gulf Polymer - Pooya Tejarat Novin Co.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Absorption <= 0.10 %ASTM D570
Melt Flow 3.8 - 4.3 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 
Chemical PropertiesOriginal ValueComments
Styrene Content <= 0.050 %Residual Monomer < 500 ppm; CLG LABPSG004 (ATOFINA TEST METHOD)
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 50.0 MPaASTM D638
Flexural Modulus 3100 MPaASTM D790
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point >= 100 °C
@Load 1.00 kg
120°C/h; ASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPERSI906 / 250310

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.