MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC LEXAN™ Copolymer EXL1413T PC/Siloxane (Americas)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Siloxane

Material Notes: LEXAN EXL1413T polycarbonate (PC) siloxane copolymer resin is a transparent injection molding grade. This resin offers excellent low temperature (-30 °C) ductility in combination with medium flow characteristics and excellent processability with opportunities for shorter IM cycle times compared to standard PC. LEXAN EXL1413T resin is a general purpose product available in transparent and opaque colors and is an excellent candidate for a broad range of applications.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.19 g/ccASTM D792
Density 1.19 g/ccISO 1183
Moisture Absorption 0.0900 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.12 %ISO 62
Linear Mold Shrinkage, Flow 0.0040 - 0.0080 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.0040 - 0.0080 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 9.0 g/10 min
@Load 1.20 kg,
Temperature 300 °C
MVR [cc/10 min]; ISO 1133
 10 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell L 89ISO 2039-2
Tensile Strength at Break 61.0 MPa50 mm/min; ISO 527
 64.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 57.0 MPa50 mm/min; ISO 527
 58.0 MPa50 mm/min; ASTM D638
Elongation at Break 124.9 %50 mm/min; ISO 527
 131.4 %50 mm/min; ASTM D638
Elongation at Yield 5.5 %50 mm/min; ISO 527
 5.8 %50 mm/min; ASTM D638
Tensile Modulus 2210 MPa50 mm/min; ASTM D638
 2350 MPa1 mm/min; ISO 527
Flexural Yield Strength 90.0 MPa2 mm/min; ISO 178
 94.0 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2150 MPa2 mm/min; ISO 178
 2210 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 890 J/mASTM D256
 795 J/m
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 65.0 kJ/m²80*10*3; ISO 180/1A
 55.0 kJ/m²
@Temperature -30.0 °C
80*10*3; ISO 180/1A
Izod Impact, Unnotched (ISO) NB80*10*3; ISO 180/1U
 NB
@Temperature -30.0 °C
80*10*3; ISO 180/1U
Charpy Impact Unnotched NBEdgew 80*10*3 sp=62mm; ISO 179/1eU
 NB
@Temperature -30.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 70.0 kJ/m²Edgew 80*10*3 sp=62mm; ISO 179/1eA
 60.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eA
Instrumented Impact Total Energy 82.0 JASTM D3763
 85.0 J
@Temperature -30.0 °C
ASTM D3763
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmASTM D257
Surface Resistance >= 1.00e+15 ohmASTM D257
Comparative Tracking Index 175 - 250 VUL 746A
Hot Wire Ignition, HWI 15 - 30 sec
@Thickness >=1.50 mm
UL 746A
 30 - 60 sec
@Thickness >=3.00 mm
UL 746A
High Amp Arc Ignition, HAI 60 - 120 arcs
@Thickness >=1.50 mm
UL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 71.5 µm/m-°C
@Temperature -40.0 - 95.0 °C
ASTM E831
 71.5 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 79.3 µm/m-°C
@Temperature -40.0 - 95.0 °C
ASTM E831
 79.3 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
Hot Ball Pressure Test 125 °CPASS; IEC 60695-10-2
Deflection Temperature at 1.8 MPa (264 psi) 118 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 124 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 141 °CRate A/50; ASTM D1525
 141 °CRate B/50; ISO 306
 142 °CRate B/120; ISO 306
UL RTI, Electrical 130 °CUL 746B
UL RTI, Mechanical with Impact 120 °CUL 746B
UL RTI, Mechanical without Impact 130 °CUL 746B
Flammability, UL94 HB
@Thickness >=0.800 mm
UL 94
 V-2
@Thickness >=2.50 mm
UL 94
Glow Wire Ignition Temperature 825 °C
@Thickness 0.800 mm
IEC 60695-2-13
 825 °C
@Thickness 1.00 mm
IEC 60695-2-13
 825 °C
@Thickness 1.50 mm
IEC 60695-2-13
 825 °C
@Thickness 2.50 mm
IEC 60695-2-13
 825 °C
@Thickness 3.00 mm
IEC 60695-2-13
Glow Wire Flammability Index 825 °C
@Thickness 0.800 mm
IEC 60695-2-12
 825 °C
@Thickness 1.00 mm
IEC 60695-2-12
 825 °C
@Thickness 1.50 mm
IEC 60695-2-12
 825 °C
@Thickness 2.50 mm
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
IEC 60695-2-12
 
Optical PropertiesOriginal ValueComments
Haze 3.0 %
@Thickness 2.54 mm
ASTM D1003
Transmission, Visible 82 %
@Thickness 2.54 mm
ASTM D1003
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 290 - 310 °CInjection Molding
Zone 1 270 - 295 °C
Zone 2 280 - 305 °CInjection Molding
Zone 3 295 - 315 °C
Melt Temperature 295 - 315 °CInjection Molding
Mold Temperature 70.0 - 95.0 °C
Drying Temperature 120 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
 48.0 hourCumulative; Injection Molding
Moisture Content 0.020 %Injection Molding
Back Pressure 0.300 - 0.700 MPa
Shot Size 40 - 60 %
Vent Depth 0.00250 - 0.00760 cm
Screw Speed 40 - 70 rpm

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH90964 / 252088

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.