MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

CoorsTek UltraSiC™ S (SC-90) Direct Sintered Silicon Carbide
Categories: Ceramic; Carbide

Material Notes:

Information provided by CoorsTek.

Key Words: DSSC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.15 g/cc0.114 lb/in³ASTM-C20
 
Mechanical PropertiesMetricEnglishComments
Hardness, Knoop 2800
@Load 0.100 kg
2800
@Load 0.221 lb
Modulus of Elasticity 410 GPa59500 ksiASTM-C848
Flexural Strength 575 MPa83400 psiASTM-F417
Compressive Strength 3500 MPa508000 psiASTM-C773
Poissons Ratio 0.210.21ASTM-C848
Fracture Toughness 4.00 MPa-m½3.64 ksi-in½KIC; Notched Beam
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity  <= 100 ohm-cm
@Temperature 1000 °C
<= 100 ohm-cm
@Temperature 1830 °F
ASTM-D1829
 <= 1000 ohm-cm
@Temperature 500 °C
<= 1000 ohm-cm
@Temperature 932 °F
ASTM-D1829
 <= 1e+05
@Temperature 25.0 °C
<= 1e+05
@Temperature 77.0 °F
ASTM-D1829
 
Thermal PropertiesMetricEnglishComments
CTE, linear 4.40 µm/m-°C
@Temperature 25.0 - 1000 °C
2.44 µin/in-°F
@Temperature 77.0 - 1830 °F
ASTM-C372
Specific Heat Capacity 0.800 J/g-°C
@Temperature 100 °C
0.191 BTU/lb-°F
@Temperature 212 °F
ASTM-E1269
Thermal Conductivity 150 W/m-K1040 BTU-in/hr-ft²-°FASTM-C408
 
Descriptive Properties
ColorBlack
Crystal Size, Average (microns)5Thin-Section
Thermal Shock Resistance, Delta;Tc, °C300Sharp decrease in fexural strength upon water quench

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

CCOOR847 / 254595

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.