MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Norplex-Micarta NP511ES Glass Epoxy Laminate  (discontinued **)
Categories: Polymer; Thermoset; Epoxy; Epoxy/Glass SMC; Filled/Reinforced Thermoset

Material Notes: NP511ES is a woven glass fabric with high temperature, static dissipative epoxy resin. It has excellent mechanical strength and electrical properties at elevated temperatures with a continuous operating temperature of 165°C.

Key Words: Micarta
Vendors: Norplex-Micarta is the leading manufacturer of high performance thermoset composite materials. We work directly with customers to manufacture the highest quality specialty sheet products, pre-pregs, rods and molded shapes, and tubes to meet demanding composite applications for our OEMs and fabricators around the world. Visit norplex-micarta.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.85 - 1.95 g/cc
@Thickness 1.57 mm
ASTM D792
Moisture Absorption at Equilibrium 0.22 %
@Thickness 1.57 mm
ASTM D229
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 100 - 120
@Thickness 1.57 mm
ASTM D785
Tensile Strength, Yield 48000 psi
@Thickness 1.57 mm
CW; ASTM D638
 60200 psi
@Thickness 1.57 mm
LW; ASTM D638
Modulus of Elasticity 4310 ksi
@Thickness 1.57 mm
CW; ASTM D229
 4780 ksi
@Thickness 1.57 mm
LW; ASTM D229
Flexural Strength 70000 psi
@Thickness 1.57 mm
CW; ASTM D790
 83000 psi
@Thickness 1.57 mm
LW; ASTM D790
Compressive Strength 85000 psi
@Thickness 12.7 mm
ASTM D695
Shear Strength 26000 psi
@Thickness 15.7 mm
ASTM D732
Izod Impact, Unnotched 9.00 ft-lb/in
@Thickness 12.7 mm
CW, Cond E-48/50; ASTM D256
 13.0 ft-lb/in
@Thickness 12.7 mm
LW, Cond E-48/50; ASTM D256
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.70 µm/m-°C
@Thickness 1.57 mm,
Temperature 20.0 °C
x-axis; IPC-TM 650-2.4.24
CTE, linear, Transverse to Flow 17.7 µm/m-°C
@Thickness 1.57 mm,
Temperature 20.0 °C
x-axis; IPC-TM 650-2.4.24
Maximum Service Temperature, Air 180 °C
Glass Transition Temp, Tg 180 °CTg
Flammability, UL94 HB
@Thickness 1.57 mm
 
Descriptive Properties
Bond Strength1800 lb0.5", ASTM D229
ColorBlack

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Goodfellow E-glass/Epoxy Composite
Hexcel® HexPly® ES 84 120°C Curing Epoxy Matrix, Aramid Balanced fabric 175 g/m2
Norplex-Micarta RT130 Epoxy Fiber Glass Laminate Tube, NEMA FR-4
Norplex-Micarta NP602 Phenolic Paper Laminate Sheet
Norplex-Micarta NP600 Phenolic Paper Laminate Sheet

PNORPN582 / 48167

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.