MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
BCC Products HPX-850 Epoxy Backfill System
Categories: Polymer; Thermoset; Epoxy

Material Notes: HPX-850 is a light weight, heat resistant, two component epoxy backfill system. Like BC 7020, the filler portion is pre-blended into the resin and hardener components for easier handling, thus simplifying the mixing process. HPX-850 features advantages such as low cost, long pot life, machineability, and low shrinkage. HPX-850 is ideally suited for numerous applications involving mold and core construction.

Information provided by BCC Products, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.820 g/cc
Linear Mold Shrinkage 0.00020 in/inASTM-D-2566-69
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 74
Ultimate Compressive Strength 4980 psi
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 285 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 24.0 hour
Pot Life 120 - 150 min1/2 lb. mass
 
Descriptive Properties
ColorBrownHardener
 Dark GrayResin
 GrayMixed
Mix ratio6:1Resin/Hardener

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBCC117 / 250982

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.