MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Amodel® A-1130 FW PPA, 30% glass fiber
Categories: Polymer; Thermoplastic; Polyphthalamide (PPA); Polyphthalamide (PPA), 30% Glass Fiber Reinforced

Material Notes: 30% glass fiber, internally lubricated, wear resistant

Amodel® A-1130 FW is a 30% glass-fiber reinforced polyphthalamide (PPA) grade containing a solid lubricant. This resin was designed for moderate-pressure, low-velocity friction and wear applications.

- Black: A-1130 FW BK 324

Markets/Uses: Wear-Resistant Plastics / High Temperature Friction & Wear / Bearing Cage

Applications: Bearings; Bushings; Filters; Gears

Features: Chemical Resistant; Creep Resistant; Good Dimensional Stability; Good Stiffness; High Strength; Low Friction; Wear Resistant

Injection notes: Storage:
- Amodel® PPA compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Amodel® PPA resins be dried prior to molding following the recommendations found in this datasheet and/or in the Amodel® PPA processing guide.

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.55 g/ccMethod A; ISO 1183
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 187 MPaISO 527-2
Elongation at Break 2.0 %ISO 527-2
Tensile Modulus 11200 MPaISO 527-2
Flexural Strength 252 MPaISO 178
Flexural Modulus 9580 MPaISO 178
 
Thermal PropertiesOriginal ValueComments
Melting Point 313 °CISO 11357-3
Deflection Temperature at 1.8 MPa (264 psi) 285 °CUnannealed; ISO 75-2/A
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 304 - 318 °C
Front Barrel Temperature 316 - 329 °C
Melt Temperature 329 - 343 °CInjection
Mold Temperature 135 °C
Drying Temperature 110 °C
@Time 14400 sec
Moisture Content 0.030 - 0.060 %Injection
 
Descriptive Properties
AdditivePTFE Lubricant
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorBlack
FormsPellets
ProcessingInjection Molding
RoHS ComplianceYes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4037 / 279837

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.