MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Tiguar® HP8FF/415 Hydroxypropyl Guar
Categories: Other Engineering Material

Material Notes: Solvay is the world’s largest producer of derivatized guar and one of the major suppliers of native guar into the Oil & Gas market. Due to their inherent properties (good viscosity, temperature stable, degradable), guar based viscosifiers are widely used in hydraulic fracturing applications. Guar products that are currently used in Oil & Gas can be divided into two major classes: native and derivatized guar. The choice of guar depends highly on the formation properties and gelling requirements. Derivatized guar offers enhanced properties in terms of hydration rate, temperature and pressure stability, and tolerance to poor water quality (salt and solids).

Information provided by Solvay

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
pH 6.850.6% guar in DI water
Viscosity 147 cP
@Temperature 30.0 °C
170s-1, 0.6%
 
Mechanical PropertiesOriginal ValueComments
Modulus of Elasticity 26.9 GPa0.6% guar, 0.5 g/L borate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Syensqo (Solvay Specialty Polymers) Tiguar® 308NB/322 Native Guar
Solvay SIPOMER® BEM Ethoxylated Behenyl Methacrylate

PSOLVAY693 / 218421

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.