MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Syensqo (Solvay Specialty Polymers) Radel® R-5000 Polyphenylsulfone (PPSU), Transparent
Categories: Polymer; Thermoplastic; Polyphenylsulfone (PPSU)

Material Notes: Transparent, general purpose for injection molding

Radel® R-5000 is a transparent polyphenylsulfone (PPSU) which offers exceptional hydrolytic stability, and toughness superior to other commercially-available, high-temperature engineering resins. This resin also offer high deflection temperatures and outstanding resistance to environmental stress cracking. Radel® polymers are inherently flame retardant, provide excellent thermal stability and possess good electrical properties.

- Smoke: Radel® R-5000 CL 301
- Amber: Radel® R-5000 NT, Radel® R-5000 XC, & Radel® R-5000 LC
- Blue: Radel® R-5000 TR BU391

Applications: Automotive Applications; Dental Applications; Food Service Applications; Hospital Goods; Medical Devices; Medical/Healthcare Applications; Membranes; Surgical Instruments

Features: Acid Resistant; Autoclave Sterilizable; Base Resistant; Biocompatible; Chemical Resistant; Detergent Resistant; E-beam Sterilizable; Ethylene Oxide Sterilizable; Flame Retardant; General Purpose; Good Dimensional Stability; Good Electrical Properties; Good Sterilizability; Good Thermal Stability; Heat Sterilizable; High ESCR (Stress Crack Resist.); High Heat Resistance; Hydrolytically Stable; Radiation (Gamma) Resistant; Radiation Sterilizable; Radiotranslucent; Steam Resistant; Steam Sterilizable; Thermal Aging Resistant; Ultra High Toughness

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.29 g/cc0.0466 lb/in³ASTM D792
Water Absorption 0.37 %
@Time 86400 sec
0.37 %
@Time 24.0 hour
ASTM D570
Water Absorption at Saturation 1.1 %1.1 %ASTM D570
Linear Mold Shrinkage, Flow 0.0070 cm/cm
@Thickness 3.18 mm
0.0070 in/in
@Thickness 0.125 in
ASTM D955
Melt Flow 14 - 20 g/10 min
@Load 5.00 kg,
Temperature 365 °C
14 - 20 g/10 min
@Load 11.0 lb,
Temperature 689 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength 69.6 MPa
@Thickness 3.18 mm
10100 psi
@Thickness 0.125 in
ASTM D638
Elongation at Break 60 - 120 %
@Thickness 3.18 mm
60 - 120 %
@Thickness 0.125 in
ASTM D638
Elongation at Yield 7.2 %
@Thickness 3.18 mm
7.2 %
@Thickness 0.125 in
ASTM D638
Tensile Modulus 2.34 GPa
@Thickness 3.18 mm
339 ksi
@Thickness 0.125 in
ASTM D638
Flexural Strength 91.0 MPa
@Strain 5.0 %,
Thickness 3.18 mm
13200 psi
@Strain 5.0 %,
Thickness 0.125 in
ASTM D790
Flexural Modulus 2.41 GPa
@Thickness 3.18 mm
350 ksi
@Thickness 0.125 in
ASTM D790
Izod Impact, Notched 6.90 J/cm
@Thickness 3.18 mm
12.9 ft-lb/in
@Thickness 0.125 in
ASTM D256
Tensile Impact Strength 399 kJ/m²
@Thickness 3.18 mm
190 ft-lb/in²
@Thickness 0.125 in
ASTM D1822
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 9.00e+15 ohm-cm9.00e+15 ohm-cmASTM D257
Dielectric Constant 3.44
@Thickness 3.18 mm,
Frequency 60 Hz
3.44
@Thickness 0.125 in,
Frequency 60 Hz
ASTM D150
Dielectric Strength >= 200 kV/mm
@Temperature 0.000 - 90.0 °C
>= 5080 kV/in
@Temperature 32.0 - 194 °F
ASTM D149
 15.0 kV/mm
@Thickness 3.18 mm
381 kV/in
@Thickness 0.125 in
ASTM D149
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 56.0 µm/m-°C
@Thickness 3.18 mm
31.1 µin/in-°F
@Thickness 0.125 in
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 207 °C
@Thickness 3.18 mm
405 °F
@Thickness 0.125 in
Unannealed; ASTM D648
Glass Transition Temp, Tg 220 °C428 °FASTM E1356
Flammability, UL94 V-0
@Thickness 0.760 mm
V-0
@Thickness 0.0299 in
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.6721.672ASTM D542
 
Processing PropertiesMetricEnglishComments
Zone 1 338 - 388 °C640 - 730 °FExtrusion
Zone 2 338 - 388 °C640 - 730 °FExtrusion
Zone 3 338 - 388 °C640 - 730 °FExtrusion
Zone 4 338 - 388 °C640 - 730 °FExtrusion
Zone 5 338 - 388 °C640 - 730 °FExtrusion
Adapter Temperature 327 - 371 °C621 - 700 °FExtrusion
Die Temperature 327 - 371 °C621 - 700 °FExtrusion
Melt Temperature 343 - 399 °C649 - 750 °FExtrusion
 360 - 391 °C680 - 736 °FInjection
Mold Temperature 138 - 163 °C280 - 325 °F
Drying Temperature  149 °C
@Time 9000 sec
300 °F
@Time 2.50 hour
 171 °C
@Time 14400 sec
340 °F
@Time 4.00 hour
Extrusion
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
ColorClear/Transparent
FormsPellets
ProcessingBlow Molding; Extrusion; Film Extrusion; Injection Molding
 Machining; Profile Extrusion; Sheet Extrusion; Thermoforming
RoHS ComplianceYes
Screw Compression Ratio2.2:1.0
Steam Sterilization> 1000 Cycles

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4392 / 280192

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.