System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Green Dot Terratek® BD3003 Biodegradable polymers
Categories:
Polymer
;
Renewable/Recycled Polymer
Material Notes:
Product Description: This resin is a proprietary blend of bio fillers, natural and synthetic biodegradable polymers. The resin is made with ingredients which pass industry standards for composting.
Information provided by Green Dot Bioplastics
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Water Vapor Transmission
16.0
g/100 in²/day
23°C, 85% RH
Oxygen Transmission Rate
58.0
cc/100 in²/day
23°C, 0% RH
Thickness
2.00
mil
Mechanical Properties
Original Value
Comments
Film Elongation at Break, MD
600 %
ASTM D882-12
Film Elongation at Break, TD
700 %
ASTM D882-12
Modulus of Elasticity
7700
ksi
MD; ASTM D882-12
7900
ksi
TD; ASTM D882-12
Film Tensile Strength at Break, MD
2600
psi
ASTM D882-12
Film Tensile Strength at Break, TD
2200
psi
ASTM D882-12
Processing Properties
Original Value
Comments
Rear Barrel Temperature
280
-
330
°F
Middle Barrel Temperature
330
-
360
°F
Front Barrel Temperature
330
-
360
°F
Die Temperature
330
-
360
°F
Melt Temperature
<=
400
°F
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
PGREEND5016 / 312287
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.