Europrene® SOL T 172 C is a radial block copolymer obtained by anionic polymerization. The polymer is based on styrene and butadiene, where bound styrene is 31 % wt. The polymer is extended with a clear paraffinic oil (45 phr). A non-staining, TNPP free antioxidant system is added during the production process. Applications: Used as a high strength base in formulated compounds for footwear and technical applications, the grade is also used in the modification of polymers and in plastic recycling.Information provided by Versalis. |