MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Ascend Performance Materials Vydyne® R550HR BK0777 PA66-GF50
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 50% Glass Fiber Filled

Material Notes: Vydyne R550HR BK0777 is a 50% glass-filled, heat-stabilized PA66 based resin designed for injection molding applications. It was specifically developed to withstand long term exposure to coolants at temperatures up to 135°C. R550HR BK0777 maintains the excellent resistance typical of PA66 in chemicals, machine and motor oils, solvents, and gasoline.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.58 g/ccDAM; ISO 1183
Water Absorption 0.72 %
@Temperature 23.0 °C,
Time 86400 sec
DAM; ISO 62
Linear Mold Shrinkage, Flow 0.0050 cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.011 cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 180 MPa50% RH; ISO 527-2
 237 MPaDAM; ISO 527-2
Elongation at Break 3.4 %DAM; ISO 527-2
 4.5 %50% RH; ISO 527-2
Tensile Modulus 14700 MPa50% RH; ISO 527-2
 15700 MPaDAM; ISO 527-2
Flexural Strength 252 MPa50% RH; ISO 178
 361 MPaDAM; ISO 178
Flexural Modulus 12300 MPa50% RH; ISO 178
 15600 MPaDAM; ISO 178
Izod Impact, Notched (ISO) 15.0 kJ/m²
@Temperature -40.0 °C
DAM; ISO 180/1A
 15.0 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 180/1A
 15.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 180/1A
 16.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 180/1A
 16.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
 18.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 180/1A
Charpy Impact Unnotched 93.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eU
 95.0 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 179/1eU
 100 kJ/m²
@Temperature -40.0 °C
DAM; ISO 179/1eU
 100 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eU
 100 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eU
 110 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eU
Charpy Impact, Notched 14.0 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 179/1eA
 15.0 kJ/m²
@Temperature -40.0 °C
DAM; ISO 179/1eA
 15.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
 17.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eA
 18.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 20.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 31.0 kV/mm
@Thickness 1.00 mm
DAM; IEC 60243
 
Thermal PropertiesOriginal ValueComments
Melting Point 260 °CDAM; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 259 °CUnannealed, 50% RH; ISO 75-2/B
 261 °CUnannealed, DAM; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 251 °CUnannealed, 50% RH; ISO 75-2/A
 254 °CUnannealed, DAM; ISO 75-2/A
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 280 - 310 °CInjection
Middle Barrel Temperature 280 - 310 °CInjection
Front Barrel Temperature 280 - 310 °CInjection
Nozzle Temperature 280 - 310 °CInjection
Melt Temperature 285 - 305 °CInjection
Mold Temperature 65.0 - 95.0 °CInjection
Drying Temperature 80.0 °C
Dry Time 4.00 hour
 
Descriptive Properties
AdditiveHeat Stabilizer
 Lubricant
AppearanceBlack
FeaturesChemical Resistant
 Corrosion Resistant
 Fatigue Resistant
 Gasoline Resistant
 High Flow
 Hydrolysis Resistant
 Laser Markable
 Lubricated
 Oil Resistant
 Organic Heat Stabilized
 Solvent Resistant
FormsPellets
Processing MethodInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PASCE9357 / 287653

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.