MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Danquinsa DANADD® 5010/20 Anti flame masterbatch
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: DANADD® 5010/20 is a highly active anti flame masterbatch. This Anti flame masterbatch is added to the PEARLTHANE® TPU’s to give them a hardly flame able equipment. The addition of these masterbatch is done either by a metering mixing unit or by a mixing in advance with the natural TPU granules.

Application: DANADD® 5010/20 serves as an anti flame masterbatch to equip the many different TPU’ s. This additive masterbatch is also compatible with polyester-, polyether- and co-polyether based TPU’s. DANADD® 5010/20 can be used for extrusion and injection molding processing. To reach a hardly flame able equipment of the materials, a high addition is necessary.

Information provided by Danquinsa GMBH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.20 g/ccDIN 53 479
 
Thermal PropertiesOriginal ValueComments
Softening Point 195 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature 185 - 215 °C
Shelf Life 6.00 Month
 
Descriptive Properties
Aspectgranules
Heat resistance by the processing10 Min240°C
Recommended mixing ratio5 – 30%

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDANQ001 / 294421

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.