System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Polytek Poly-Optic® 1410 Rigid Clear Polyurethane
Categories:
Polymer
;
Thermoset
;
Polyurethane, TS
Material Notes:
A versatile, clear polyurethane. A matte finish will give a frosted appearance, and a higher gloss will increase its transparency.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
1.07
g/cc
Brookfield Viscosity
700
cP
Mixed
Mechanical Properties
Original Value
Comments
Hardness, Shore D
80
Tensile Strength
4566
psi
7870
psi
Post cured for 16 hours at 160°F
Elongation at Break
12 %
Post cured for 16 hours at 160°F
27 %
Modulus of Elasticity
127.5
ksi
Post cured for 16 hours at 160°F
96830
ksi
Flexural Strength
4893
psi
@Strain 5.0 %
10640
psi
@Strain 5.0 %
Post cured for 16 hours at 160°F
Flexural Modulus
144000
psi
241500
psi
Post cured for 16 hours at 160°F
Thermal Properties
Original Value
Comments
Deflection Temperature at 0.46 MPa (66 psi)
100
°F
149
°F
Post cured for 16 hours at 160°F
Processing Properties
Original Value
Comments
Cure Time
168
hour
Pot Life
15.0
min
Descriptive Properties
Color / Appearance
Water clear
Part A
Water clear
Part B
Demold Time (hrs)
2
1- inch thick
Max Exotherm (°F)
265
1-lb mass
Mix Ratio by weight
3 to 2
Part A to Part B
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
PPOLYT9908 / 287688
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.