Compound 19741 is a 70 durometer salmon colored Silicone elastomer, it is formulated with FDA sanctioned materials to meet the 3A Sanitary specifications. It exhibits good resistance to heat and will remain non brittle at very low temperatures. This compound will meet or exceed the specifications listed and has the following physical properties: ASTM D2000 3 FC 710 A19 B37 EO16 EA14 F1-11 G11; 5 GE 709 A19 EA14 EO16 EO36 F19; 7 GE 707 A19 EA14 EO16 EO36 F19; 6 GE 704 A19 EA14 EO16 EO36 F19 3 A Sanitary Standards Class I, II, III & IVInformation provided by Pressure Seals Inc. |