MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
HB Fuller Flexel™ FN1000 Film Adhesive
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: FN1000 is a reactive, low temperature heat-activated, reactive adhesive film for bonding similar and dissimilar plastic substrates like ABS, PC, PBT, pre-treated Olefins (low surface energy plastics), Polyamide, Polyimide, engineering plastics, SMC, FRP, GRP, and advanced composites. FN1000 is also very effective at bonding PET films, textiles, artificial and genuine leather.

Features and Benefits:

  • Low temperature, easy application method
  • Excellent adhesion to plastics, textiles, leather, and good adhesion to metals
  • High fracture toughness, peel and shear strength while maintaining flexibility
  • High heat resistance and chemical resistance after cure
  • Halogen free as defined by IEC 61249-2-21
  • High bond strength on a variety of substrates
  • VOC Emission free
  • Low thermal expansion coefficient

Information provided by H.B. Fuller Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.12 g/cc
Solids Content 100 %
Storage Temperature <= 30.0 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 26.0 MPaBonded at 90ºC for 60 sec
Elongation at Break 550 %Bonded at 90ºC for 60 sec
Tensile Modulus 180 MPaYoung’s, Bonded at 90ºC for 60 sec
 
Thermal PropertiesOriginal ValueComments
Glass Transition Temp, Tg -46.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
 
Descriptive Properties
ColorMilky White
ConsistencyNon-Tack Film

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHBFULL224 / 317015

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.