Unimoll® AGF (RT) is a yellowish mixture of glycerin acetates. The plasticizer Unimoll® AGF (RT) is compatible with a various polymers, especially PVC. Unimoll® AGF (RT) is developed for applications in contact with food including PVC cling films. Chemical composition: mixture of glycerin acetates Applications: Unimoll® AGF (RT) was developed for plasticizing films which get in contact with food stuffs. This product is also used for other PVC applications. Unimoll® AGF (RT) is used when regulations and recommendations governing food contacting applications need to be met. Information provided by Lanxess. |