MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Teknor Apex Medalist® MD-53283 Thermoplastic Elastomer
Categories: Polymer; Thermoplastic; Elastomer, TPE

Material Notes: Notes: Medalist MD-53200 series is a high performance thermoplastic elastomer series, designed to be a sustainable alternative to flexible PVC for medical tubing and film. Medalist MD-53283 is a higher hardness, low density, clear, lubricated grade, available in Nat and color-matched, intended for use in medical and healthcare applications, with excellent processability and throughput in extruded tubing.

Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America

Features: Autoclave Sterilizable; Chemical Resistant; Ethylene Oxide Sterilizable; Good Adhesion; Good Colorability; Good Flexibility; Good Processability; Good Sterilizability; Good Toughness; Halogen Free; High Clarity; High Hardness; High Purity; Kink Resistant; Low Density; Low Specific Gravity; Lubricated; Radiation (Gamma) Resistant

Uses: Clear Sheet; Film; Hose; Medical/Healthcare Applications; Pharmaceuticals; Rubber Replacement; Tubing

Agency Ratings: ISO 10993 Part 5; ISO 13485

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Cast Film; Extrusion; Injection Molding

Preliminary data. Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.890 g/cc0.0322 lb/in³ASTM D792
Melt Flow 8.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
8.0 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  84
@Time 5.00 sec
84
@Time 0.00139 hour
ASTM D2240
 86
@Time 1.00 sec
86
@Time 0.000278 hour
ASTM D2240
Tensile Strength at Break 14.5 MPa2100 psiASTM D412
Tensile Stress at Strain  5.17 MPa
@Strain 50 %
750 psi
@Strain 50 %
ASTM D412
 5.52 MPa
@Strain 100 %
800 psi
@Strain 100 %
ASTM D412
 27.9 MPa
@Strain 300 %
4050 psi
@Strain 300 %
ASTM D412
Elongation at Break 650 %650 %ASTM D412
Tear Strength 77.1 kN/m440 pliASTM D624
 
Processing PropertiesMetricEnglishComments
Processing Temperature 193 - 227 °C380 - 440 °FMelt, Injection
Rear Barrel Temperature 149 - 171 °C300 - 340 °FInjection
Middle Barrel Temperature 171 - 193 °C340 - 380 °FInjection
Front Barrel Temperature 193 - 227 °C380 - 440 °FInjection
Nozzle Temperature 193 - 227 °C380 - 440 °FInjection
Zone 1 160 - 188 °C320 - 370 °FExtrusion
Zone 2 182 - 196 °C360 - 385 °FExtrusion
Zone 3 182 - 204 °C360 - 400 °FExtrusion
Zone 4 182 - 204 °C360 - 400 °FExtrusion
Zone 5 182 - 210 °C360 - 410 °FExtrusion
Adapter Temperature 177 - 216 °C350 - 420 °FExtrusion
Die Temperature 177 - 216 °C350 - 420 °FExtrusion
Mold Temperature 21.1 - 51.7 °C70.0 - 125 °FInjection
Back Pressure 0.345 - 1.03 MPa50.0 - 150 psiInjection
Cushion 0.356 - 2.54 cm0.140 - 1.00 inInjection
Screw Speed 30 - 100 rpm30 - 100 rpmExtrusion
 50 - 100 rpm50 - 100 rpmInjection
 
Descriptive Properties
AppearanceClear/Transparent
 Colors Available

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ0748 / 237239

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.