MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

RAMPF RAKU® TOOL IE-3285 Polyurethane, polyether based elastomer
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyether Grade

Material Notes: Flexible polyurethane / polyether based elastomer

Key Properties:

  • Excellent physical properties after RT cure
  • Free of mercury, MOCA or TDI
Applications:
  • For hand-batch processing
Cure 1: 7 days at 77°F

Information provided by © RAMPF Tooling Solutions GmbH & Co. KG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.08 g/cc0.0390 lb/in³Cure 1; ASTM D-792
 1.12 g/cc0.0405 lb/in³Resin; ASTM D-792
 1.16 g/cc0.0419 lb/in³Hardener; ASTM D-792
Viscosity 200 cP200 cPHardener; ASTM D-2393
 3100 cP3100 cPMix; ASTM D-2393
 3300 cP3300 cPResin; ASTM D-2393
Linear Mold Shrinkage 0.0010 - 0.0020 cm/cm0.0010 - 0.0020 in/inCure 1; ASTM D-2566
Storage Temperature 15.0 - 30.0 °C59.0 - 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 75 - 8575 - 85Cure 1; ASTM D-2240
Tensile Strength 8.96 MPa1300 psiCure 1; ASTM D-638
Elongation at Break 280 %280 %Cure 1; ASTM D-638
Tear Strength 35.1 kN/m200 pliCure 1; ASTM D-624
 
Processing PropertiesMetricEnglishComments
Cure Time 180 - 300 min3.00 - 5.00 hourMix, Demold time
Gel Time 20.0 - 30.0 min20.0 - 30.0 minMix
 
Descriptive Properties
AspectBlackCure 1
Mix Ratio100:13Resin: Hardener, Weight
 100:13Resin: Hardener, Volume

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRAMPF036 / 317636

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.