MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Lubrizol Advanced Materials X-5490 Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: X-5490 is a Polycarbonate compound with carbon nanotube added for enhanced electrical, mechanical and cleanliness performance. Available in pellet form for injection molding applications, It solves a wide range of electrostatic discharge problems. Applications: Hard disk drive component trays; Media cassettes
Availability: Asia Pacific, Europe, Latin America, North America
Additive: Carbon Nano
Features: Durable; Consistent performance; Good Electrical Properties; Rapid Static Decay; Recyclable Material
Uses: Electrical/Electronic Applications; Computer Components
Appearance: Black
Forms: Pellets
Processing Method: Injection Molding

Information provided by Lubrizol Advanced Materials, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ASTM D792
Linear Mold Shrinkage, Flow 0.0050 - 0.0080 cm/cm0.0050 - 0.0080 in/inASTM D955
Melt Flow 23 g/10 min
@Load 5.00 kg,
Temperature 300 °C
23 g/10 min
@Load 11.0 lb,
Temperature 572 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 52.4 MPa7600 psiASTM D638
Elongation at Break 17 %17 %ASTM D638
Tensile Modulus 2.00 GPa290 ksiASTM D638
Flexural Modulus 2.86 GPa415 ksiASTM D790
Izod Impact, Notched 1.60 J/cm3.00 ft-lb/inASTM D256
 
Electrical PropertiesMetricEnglishComments
Static Decay 0.10 sec0.10 sec1000 V to 10 V
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 136 °C277 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 111 °C232 °FUnannealed; ASTM D648
 
Descriptive Properties
Ionic Content1 ng/cm2Anions Cl, Test Method #3010-4
 1 ng/cm2Anions SO4, Test Method #3010-4
Outgassing0.00 ng/gAcrylates, Test Method #3010-3
 16.0 ng/gToluene, Test Method #3010-3
 3.00 ng/gStyrene, Test Method #3010-3
 88.0 ng/gTotal Organics, Test Method #3010-3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PLUBR6012 / 268314

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.