Product Description: - A formulated clarity film resin for thing gauge optical packaging
- Optimum gauge range: 0.8-2.5 mil
Complies with: US FDA 21 CFR 177.1520©2.2a; EU NO 10/2011. Consult the regulations for complete details.Availability: North America Additive: Antiblock: No; Processing Aid: No; Slip: No Agency Ratings: DMF; FDA 21 CFR 177.1520©2.2; EU NO 10/2011 Form: Pellets Processing Method: Blown Film; Cast Film Information provided by The Dow Chemical Company |