MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Danquinsa MORCHEM UD 5152HR Polyurethane dispersion
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyester Grade

Material Notes: MORCHEM UD 5152HR is a application ready, aqueous, aliphatic structured polyester urethane dispersion. This fast crystalline polyurethane dispersion distinguish itself by its extreme good adhesion on polyester and polyether foam as well as through its high adhesive strength on polyester fabrics. The aliphatic based PU dispersion is acting for the production of shoe adhesives as well as for the production of textile and leather finishes.

Application: MORCHEM UD 5152HR is applied to serve as a basic raw material by the production of aqueous 1- and 2-component adhesives. Adhesives and adhesive coatings which were produced with MORCHEM UD 5152HR are especially good suitable for:

  • Textile lamination
  • Coating of casings and profiles
  • Lamination of thermoplastic foils with wooden materials as for instance by membrane press application
  • Deep-draw and press lamination application for the automotive industry.
  • Shoe soles- and shoe shank fitting
  • Lamination of split leather and plastic foils.
We recommend, for the processing of 2- component adhesives, the application of the cross link agent DANCURE 101.

Information provided by Danquinsa GMBH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 40 %
pH 7.0 - 9.5
Viscosity 30 - 250 cP
Storage Temperature 5.00 - 25.0 °C
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 45.0 MPaDIN 53.504
Elongation at Break 450 %DIN 53.504
100% Modulus 23.0 MPaDIN 53.504
300% Modulus 35.0 MPaDIN 53.504
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
 
Descriptive Properties
AspectMilky, white liquid
Composition< 2% N-Methyl-2-PyrrolidoneResidual solvent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDANQ188 / 294608

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.