A fast cure 100% solids hot spray applied coating system designed to produce a tough, impact resistant surface designed for expanded polystyrene (EPS) and polyurethane foam. RECOMMENDED APPLICATIONS: Internal and external protection of EPS and PU foam especially where FR performance is essential. Various FR certification available. FEATURES: • No primer required onto EPS or PU foam. • Fast cure for increased productivity • Zero VOC’s. Information provided by ITW Performance Polymers. |