MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Lubrizol Advanced Materials Stat-Rite® S-506 High Impact Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene, Impact Modified

Material Notes: Product Description: S-506 is a static dissipative High-Impact Polystyrene alloy. It utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to enhance standard HIPS packaging sheet with a layer of clean, permanent ESD protection. Used as a skin layer, Stat-Rite® S-506 provides more consistent ESD protection than coatings and anti-stat. The Stat-Rite® skin will NOT wash off or deteriorate over time, providing reliable ESD protection for many years. Features: More permanent than anti-stat; Provides protection for many years; Cleaner than anti-stat, coatings or carbon-filled sheet; More consistent than anti-stat or coatings. Applications: Static dissipative layer on HIPS electronics packaging.
Availability: Asia Pacific, Europe, Latin America, North America
Features: Antistatic; Clean/High Purity; Durable; ESD Protection; Rapid Static Decay; Wear Resistant
Uses: Electrical/Electronic Applications; Packaging
Appearance: Yellow
Forms: Pellets

Information provided by Lubrizol Advanced Materials, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.07 g/ccASTM D792
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 210 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 3000 psiMeasured on a co-extruded ABA sheet of S506/HIPS/S506 in a 10/80/10 thickness ratio; ASTM D638
Elongation at Break 85 %Measured on a co-extruded ABA sheet of S506/HIPS/S506 in a 10/80/10 thickness ratio; ASTM D638
Tensile Modulus 200000 psiMeasured on a co-extruded ABA sheet of S506/HIPS/S506 in a 10/80/10 thickness ratio; ASTM D638
Flexural Modulus 200000 psiMeasured on a co-extruded ABA sheet of S506/HIPS/S506 in a 10/80/10 thickness ratio; ASTM D790
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 1.00e+9 ohm12% RH, Measured on a co-extruded ABA sheet of S506/HIPS/S506 in a 10/80/10 thickness ratio; ESD S11.11
Surface Resistivity per Square 3.00e+9 ohm50% RH, Measured on a co-extruded ABA sheet of S506/HIPS/S506 in a 10/80/10 thickness ratio; ASTM D257
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 167 °FUnannealed, Measured on a co-extruded ABA sheet of S506/HIPS/S506 in a 10/80/10 thickness ratio; ASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLUBR6024 / 268326

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.