MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Copper Alloy, UNS C42300, H04 Temper, Sheet & Strip
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Hard

Fabrication Properties: Excellent Suitability – Soldering, Capacity for Being Cold Worked; Good Suitability – Gas Shielded Arc Welding, Butt Weld, Capacity for Being Hot Formed; Fair Suitability – Oxyacetylene Welding

Typical Uses: Electrical terminals; Relay Elements; Terminals Connectors

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 8.94 g/cc0.323 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Vickers 187
@Load 3.00 kg
187
@Load 6.62 lb
Tensile Strength >= 580 MPa>= 84100 psi
 621 MPa90100 psiTypical
Tensile Strength, Yield 592 MPa85900 psi0.2% Offset, Typical
 550 - 640 MPa79800 - 92800 psi0.2% Offset
Elongation at Break 4.0 %4.0 %
Tensile Modulus 120 GPa17400 ksi
Modulus of Rigidity 45.86 GPa6651 ksiCalculated
Poissons Ratio 0.3080.308
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.00000540 ohm-cm0.00000540 ohm-cm32% IACS
 
Thermal PropertiesMetricEnglishComments
Melting Point 1012 - 1020 °C1854 - 1868 °F
Solidus 1012 °C1854 °F
Liquidus 1020 °C1868 °F
 
Component Elements PropertiesMetricEnglishComments
Copper, Cu 87 - 91 %87 - 91 %
Lead, Pb <= 0.010 %<= 0.010 %
Nickel, Ni 0.50 - 1.5 %0.50 - 1.5 %
Silicon, Si 0.10 - 0.30 %0.10 - 0.30 %
Tin, Sn 0.50 - 1.5 %0.50 - 1.5 %
Zinc, Zn 5.7 - 11.9 %5.7 - 11.9 %As Balance
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

MC42300x1 / 291931

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.