MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
BASF Ultradur® B 4441 G5 PBT, 25% Glass Fiber Reinforced
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), 30% Glass Fiber Filled

Material Notes: Ultradur B 4441 G5 is a 25% glass reinforced injection molding PBT optimized for glow wire requirements. For parts requiring enhanced fire resistance. (Halogen and Antimony free)

Applications: Typical applications include components for household appliances, connectors, and power switches.

Information provided by BASF.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.53 g/ccISO 1183
Moisture Absorption 0.200 %50% RH; ISO 62
Water Absorption at Saturation 0.40 %ISO 62
Viscosity Test 105 cm³/gISO 1628
Linear Mold Shrinkage, Flow 0.0040 cm/cmISO 294-4
Linear Mold Shrinkage, Transverse 0.0124 cm/cmISO 294-4
Melt Flow 15 g/10 min
@Load 2.16 kg,
Temperature 275 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 110 MPaISO 527
Elongation at Break 2.3 %ISO 527
Tensile Modulus 9800 MPaISO 527
Flexural Strength 180 MPaISO 178
Flexural Modulus 10000 MPaISO 178
Charpy Impact Unnotched 45.0 kJ/m²
@Temperature 23.0 °C
ISO 179
 47.0 kJ/m²
@Temperature -30.0 °C
ISO 179
Charpy Impact, Notched 7.00 kJ/m²ISO 179
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmIEC 60093
Surface Resistance >= 1.00e+16 ohmIEC 60093
Dielectric Constant 3.6
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.0137
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 525 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
Melting Point 223 °CISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 220 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 210 °CISO 75
UL RTI, Electrical 140 °C
@Thickness 1.50 mm
UL746B
Flammability, UL94 V-0
@Thickness 0.400 mm
 5VA
@Thickness 1.50 mm
 
Processing PropertiesOriginal ValueComments
Melt Temperature 250 - 270 °C
Mold Temperature 60.0 - 100 °C
Drying Temperature 100 - 120 °C
@Time 14400 sec
Moisture Content <= 0.040 %
Injection Pressure 500 - 1500 psi

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBASF8909 / 254867

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.