MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

Mitsubishi FGF Recycled PLA MATT 3D Printing Polymer
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Renewable/Recycled Polymer; Thermoplastic; Polylactic Acid (PLA) Biopolymer

Material Notes: FGF Recycled PLA MATT is an easy to print variant on the everyday material PLA, with an aesthetical matt effect. Its surface diffuses light to give it a matt look and creates a rough feeling. PLA MATT is slightly abrasive, please consider using a hardened nozzle.

Features:

  • Matt effect, low light refraction
  • Easy to print rough surface
  • Reliable bed adhesion
  • Improved printing speed compared to PLA
Colors on request.

Information provided by Mitsubishi Chemical.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.38 g/cc1.38 g/ccISO 1183
Linear Mold Shrinkage 0.00090 cm/cm0.00090 in/inISO 294
Melt Flow 32.3 g/10 min
@Load 5.00 kg,
Temperature 200 °C
32.3 g/10 min
@Load 11.0 lb,
Temperature 392 °F
ISO 1133
Storage Temperature 15.0 - 25.0 °C59.0 - 77.0 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 50.0 MPa7250 psiISO 527
Tensile Strength, Yield 47.0 MPa6820 psiISO 527
Elongation at Break 1.8 %1.8 %ISO 527
Elongation at Yield 2.2 %2.2 %ISO 527
Tensile Modulus 5.75 GPa834 ksiISO 527
Charpy Impact, Notched 0.190 J/cm²0.904 ft-lb/in²ISO 179
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 58.0 °C136 °FISO 306
 
Processing PropertiesMetricEnglishComments
Zone 1 160 - 200 °C320 - 392 °F
Zone 2 170 - 210 °C338 - 410 °F
Zone 3 180 - 220 °C356 - 428 °F
Die Temperature 190 - 230 °C374 - 446 °F
Drying Temperature 50.0 °C122 °F<250 ppm
Dry Time 6.00 hour6.00 hour
 
Descriptive Properties
Mass Temperature209°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMITS9823 / 301048

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.