A polyolefin-based, mineral filled, thermo-elastoplastic composite material. Contains modified additives, thermostabilizers and light-stabilizers. Displays a high resistance to ozone and atmosphere, to aggressive environments and polar solvents. Designed for isolation materials manufacture and protective shells for cables and wires; rubbers exploited in a temperature range of -60 °C – 90 °C (capable to withstand a short heat to 105 °C). Unlike rubbers, this material is capable to endure many recycles, along with dye with super concentrates in the process of product manufacture. Available in natural and black colors.Information provided by Polyplastic Compounds |