MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Danquinsa DANADD® LFC Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: DANADD® LFC is a very high quality and very effective additive compound which is added to the thermoplastic polyurethane granules (TPU’s) out of the PEARLTHANE® – range to adjust the electrical conductibility. This thermoplastic additive compound is available in form of granules and will be added with the help of an masterbatch metering unit or by addition into the TPU granules by the use of a tumble mixer. Because of the heat conduction is this special compound is supporting the melt homogenization and the distribution of heat in the extruder.

Application: DANADD® LFC is added to the TPU’s which will be processed by injection moulding to produce conductive wheels and castors, sealants and many various technical parts. This special additive is added directly by the extrusion of TPU foils to give them a conductive equipment. The addition to the TPU is depending on the electrical conductive requirements. Normally 5 to 30% will be added from this special additive batch to the divers TPU’s of the PERALTHANE® - range.

Information provided by Danquinsa GMBH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.32 g/ccDIN 51.757
Storage Temperature 15.0 - 25.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
 
Descriptive Properties
Aspectsilver colored to grey granule
Dosage5-30%
Heat resistance<500°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDANQ008 / 294428

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.