MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Ascend Performance Materials HiDura™ S3MG30H BK0835 Nylon PA610-GF30
Categories: Polymer; Renewable/Recycled Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 610 (PA610); Nylon 610, Glass Reinforced

Material Notes: HiDura S3MG30H BK0835 is a 30% glass fiber reinforced, heat stabilized polyamide 610 with 42% bio-based content for injection molding applications.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.31 g/ccDAM; ISO 1183
Water Absorption 0.40 %
@Temperature 23.0 °C,
Time 86400 sec
DAM; ISO 62
Moisture Absorption at Equilibrium 1.0 %DAM to 50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0060 cm/cm
@Thickness 2.00 mm
DAM; ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 120 MPa50% RH; ISO 527-2
 158 MPaDAM; ISO 527-2
Elongation at Break 4.4 %DAM; ISO 527-2
 7.6 %50% RH; ISO 527-2
Tensile Modulus 6800 MPa50% RH; ISO 527-2
 9100 MPaDAM; ISO 527-2
Flexural Strength 152 MPa50% RH; ISO 178
 215 MPaDAM; ISO 178
Flexural Modulus 6200 MPa50% RH; ISO 178
 8400 MPaDAM; ISO 178
Poissons Ratio 0.38ISO 527-2
Izod Impact, Notched (ISO) 12.0 kJ/m²
@Temperature -40.0 °C
DAM; ISO 180/1A
 12.0 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 180/1A
 13.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 180/1A
 13.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 180/1A
 16.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
 18.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 180/1A
Charpy Impact Unnotched 87.0 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 179/1eU
 87.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eU
 96.0 kJ/m²
@Temperature -40.0 °C
DAM; ISO 179/1eU
 97.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eU
 97.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eU
 102 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eU
Charpy Impact, Notched 11.0 kJ/m²
@Temperature -40.0 °C
DAM; ISO 179/1eA
 12.0 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 179/1eA
 13.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
 13.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eA
 18.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 20.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 29.0 kV/mm
@Thickness 1.00 mm
50% RH; IEC 60243
 32.0 kV/mm
@Thickness 1.00 mm
DAM; IEC 60243
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 21.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
DAM; ISO 11359-2
CTE, linear, Transverse to Flow 120 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
DAM; ISO 11359-2
Melting Point 225 °CDAM; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 216 °CUnannealed, 50% RH; ISO 75-2/B
 219 °CUnannealed, DAM; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 193 °CUnannealed, 50% RH; ISO 75-2/A
 197 °CUnannealed, DAM; ISO 75-2/A
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 245 - 275 °CInjection
Middle Barrel Temperature 265 - 290 °CInjection
Front Barrel Temperature 270 - 300 °CInjection
Nozzle Temperature 275 - 305 °CInjection
Melt Temperature 255 - 300 °CInjection
Mold Temperature 70.0 - 100 °CInjection
Drying Temperature >= 80.0 °C
Dry Time >= 4.00 hour
 
Descriptive Properties
AdditiveHeat Stabilizer
Agency RatingsASTM, D4066 PA0720A4306
 ASTM, D6779 PA0000A4356
 ISO, 1043 PA610 GF30
AppearanceBlack
FeaturesChemical Resistant
 Oil Resistant
 Solvent Resistant
FormsPellets

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PASCE8609 / 293358

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.