SBR 1778 is a general-purpose cold polymerized, naphthenic oil-extended elastomer. It exhibits excellent UV light stability for a SBR polymer. Unique Features: - Cold polymerized styrene-butadiene elastomer
- Ultraviolet light stability
- Naphthenic oil extended for improved processing
Applications:- Coating fabrics
- White sidewalls and tires carcasses
- Footwear and mechanical rubber goods
Information provided by Lion Elastomer |