- detectable via metal detector
- x-ray detectable
- Explanation of food contact according to FDA and EU 10/2011 on request
- good toughness
- low water absorption
- good chemical resistance
Target Industries:former material REZ-RS-3943Information provided by Ensinger Inc. |