MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Dow Dow™ DNDA-9820 NT7 LLDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Injection Molded

Material Notes: Product Description: Dow GRSN-9820 NT7 linear low density polyethylene resin is produced using UNIPOL™ PE Process Technology and is supplied in granular form. This resin is specifically designed as a carrier resin for color concentrates and other masterbatch systems. The fine particle size reduces the need for grinding, and the high surface area of granular resin allows for more uniform dispersion of concentrate in the final product. GRSN-9802 NT7 is compatible with polyethylene and polypropylene resins and can be used in a wide variety of fabrication processes.
Overview:
  • Granular form
  • Carrier resin for masterbatch systems
Complies with: US FDA 21 CFR 177.1520©3.2a; EU No 10/2011. Consult the regulations for complete details.

Availability: North America

Additive: Antiblock: No; Processing Aid: No; Slip: No

Agency Ratings: US FDA 21 CFR 177.1520©3.2a; EU No 10/2011

Form: Granules

Information provided by The Dow Chemical Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.926 g/ccASTM D792
ESCR 100% Igepal® 20 hour
@Temperature 50.0 °C
F50; ASTM D1693
Melt Flow 20 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 50ASTM D2240
Tensile Strength at Break 1100 psiASTM D638
Tensile Strength, Yield 1700 psiASTM D638
Elongation at Break 60 %ASTM D638
Elongation at Yield 3.0 %ASTM D638
Flexural Modulus 560000 psi2% Secant; ASTM D790B
Tensile Impact Strength 43.0 ft-lb/in²Type S; ASTM D1822
 
Thermal PropertiesOriginal ValueComments
Melting Point 253 °F
Crystallization Temperature 226 °FPeak
Deflection Temperature at 0.46 MPa (66 psi) 109 °FUnannealed; ASTM D648
Vicat Softening Point 201 °FASTM D1525
Brittleness Temperature -105 °FASTM D746

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDOWF485 / 311178

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.