This metallocene linear low density polyethylene is an ethylene-hexene copolymer tailored for blown film applications that require: • Good tensile properties • Exceptional toughness• Surface printing • Stiffness. Typical blown film applications include: • Heavy duty packaging • Industrial packaging • Institutional packaging. information provided by Chevron Phillips Chemical Company LP. |