MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Designer Molecules PEAM-1769 Polyester acrylate/methacrylate
Categories: Polymer; Adhesive

Material Notes: Description: PEAM-1769 is a polyester acrylate/methacrylate that exhibits excellent adhesion, low warpage, and hydrophobicity. The oligomer has very high thermal stability and low volatility. It can be used as a base oligomer in a formulation or an additive.

Highlights:

  • Ultra low modulus
  • Thermal stability
  • Hydrophobic
  • Adhesion to metals
  • High adhesion to various substrates
  • Flexibilizer

Information provided by Designers Molecules

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 20000 cP20000 cPHaake Rheometer
Molecular Weight 1769 g/mol1769 g/mol
Storage Temperature <= 10.0 °C<= 50.0 °F
 
Mechanical PropertiesMetricEnglishComments
Tensile Modulus  0.00100 GPa
@Temperature 150 °C
0.145 ksi
@Temperature 302 °F
cured with 2% Dicumyl Peroxide
 0.0480 GPa
@Temperature 25.0 °C
6.96 ksi
@Temperature 77.0 °F
cured with 2% Dicumyl Peroxide
 1.30 GPa
@Temperature -65.0 °C
189 ksi
@Temperature -85.0 °F
cured with 2% Dicumyl Peroxide
 
Thermal PropertiesMetricEnglishComments
CTE, linear 110 µm/m-°C61.1 µin/in-°Foc 1, cured with 2% Dicumyl Peroxide
 250 µm/m-°C139 µin/in-°Fco 2, cured with 2% Dicumyl Peroxide
Glass Transition Temp, Tg -40.0 °C-40.0 °FTMA, cured with 2% Dicumyl Peroxide
 -10.0 °C14.0 °FDMA, cured with 2% Dicumyl Peroxide
Decomposition Temperature >= 375 °C>= 707 °F
 
Descriptive Properties
AppearanceAmber liquid
Weight Loss<3.0%@ 300°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PDESGN016 / 255380

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.