MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Evonik VESTOWAX® C 40 Fischer-Tropsch Wax
Categories: Polymer

Material Notes: Synthetic Waxes: With its VESTOWAXR product range Evonik offers synthetic waxes produced by Fischer-Tropsch-Process. This process yields straight-chain products possessing low viscosity in the melt and having molecular weights of between 500 and 1,000 g/mol. The definition of the term ›wax‹ is based less on the chemical composition of a substance than on its physical properties:
  • kneadable at 20 °C, with a consistency ranging from solid to brittle-hard
  • coarsely to finely crystalline, translucent to opaque
  • melt above 40 °C without decomposition
  • already of relatively low viscosity at just above the melting point
  • highly temperature-dependent consistency and solubility
  • can be polished under gentle pressure
In addition to crude FT-wax, the range of VESTOWAXR products includes modified hard paraffins, oxidates and partially saponified waxes. Depending on the supply form different bags sizes are offered: Prills and micro prills usually in 25 kg bags or 700 kg big bags, pellets, flakes and coarse powder usually in 20 kg bags, microfine powder usually in 15 kg bags.

Your benefits:

  • solutions for a multitude of applications
  • extensive range of FT-modified grades
  • wide variety of supply forms- from pellets to microfine powder

Information provided by Evonik

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.960 g/ccDIN 53 479
Viscosity <= 20 cP
@Temperature 130 °C
DIN 52 007/1
 
Chemical PropertiesOriginal ValueComments
Total Acid Number 24 - 27[mg KOH/g]; ASTM D 1386
 
Mechanical PropertiesOriginal ValueComments
Penetration P(0), 1/10 mm 2.0 - 4.0ASTM D1321
 
Thermal PropertiesOriginal ValueComments
Dropping Point 102 - 108 °CASTM D566
 
Descriptive Properties
AppearanceWhite
Saponification Number40-50 mg KOH/mgASTM D1387

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Yparex 8305 Polyolefin Adhesive Resin (European Grade)
Phillips 66 ISO Grade 46 Heat Transfer Oils
Innospec VISCOWAX® 111 PE-Wax
Honeywell Rheolub® RL-315 Wax Blend
Honeywell A-C® 6A Low Density PE homopolymer

PEVONIL129 / 196333

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.