MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

RAMPF RAKU® TOOL InnoTuf® HP-2140 Polyurethane, polyether based elastomer
Categories: Polymer; Thermoplastic; Polyurethane, TP; Thermoplastic Polyurethane (TPUR), Polyether Grade

Material Notes: High performance polyether based polyurethane elastomer

Key Properties:

  • Excellent physical properties after RT cure
  • Free of mercury, MOCA or MDI
Applications:
  • For hand-batch processing methods
Cure 1: 7 days at 77°F
Cure 2: 24 hours at 77°F + 5 hours at 150°F

Information provided by © RAMPF Tooling Solutions GmbH & Co. KG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.03 g/cc0.0372 lb/in³Hardener; ASTM D-792
 1.04 g/cc0.0376 lb/in³Cure 1; ASTM D-792
 1.04 g/cc0.0376 lb/in³Cure 2; ASTM D-792
 1.06 g/cc0.0383 lb/in³Resin; ASTM D-792
Viscosity 125 cP125 cPHardener; ASTM D-2393
 475 cP475 cPMix; ASTM D-2393
 625 cP625 cPResin; ASTM D-2393
Linear Mold Shrinkage 0.0020 - 0.0050 cm/cm0.0020 - 0.0050 in/inCure 1; ASTM D-2566
 0.0020 - 0.0050 cm/cm0.0020 - 0.0050 in/inCure 2; ASTM D-2566
Storage Temperature 15.0 - 30.0 °C59.0 - 86.0 °F
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 35 - 4535 - 45Cure 1; ASTM D-2240
 35 - 4535 - 45Cure 2; ASTM D-2240
Tensile Strength 4.14 MPa600 psiCure 1; ASTM D-638
 4.31 MPa625 psiCure 2; ASTM D-638
Elongation at Break 480 %480 %Cure 1; ASTM D-638
 500 %500 %Cure 2; ASTM D-638
Tear Strength 16.7 kN/m95.0 pliCure 1; ASTM D-624
 18.4 kN/m105 pliCure 2; ASTM D-624
 
Processing PropertiesMetricEnglishComments
Cure Time 300 - 420 min5.00 - 7.00 hourMix, Demold time
Gel Time 20.0 - 30.0 min20.0 - 30.0 minMix
 
Descriptive Properties
AspectLight AmberCure 1
 Light AmberCure 2
Mix Ratio100:47Resin: Hardener, Weight
 100:50Resin: Hardener, Volume

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PRAMPF095 / 317695

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.