MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Syensqo (Solvay Specialty Polymers) Solef® 31508/0009 PVDF
Categories: Polymer; Thermoplastic; Fluoropolymer; Polyvinylidene Fluoride (PVDF); Polyvinylidinefluoride (PVDF), Molded/Extruded

Material Notes: Solef® 31508/0009 PVDF copolymer is a low viscosity and very flexible grade for Wire & Cable applications.

Applications: Wire & Cable Applications

Features: Copolymer; Good Flexibility; Low Viscosity

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.75 - 1.80 g/cc0.0632 - 0.0650 lb/in³ASTM D792
Water Absorption <= 0.040 %
@Time 86400 sec
<= 0.040 %
@Time 24.0 hour
ASTM D570
Linear Mold Shrinkage, Flow 0.020 - 0.030 cm/cm0.020 - 0.030 in/inASTM D955
Melt Flow 3.0 - 8.0 g/10 min
@Load 2.16 kg,
Temperature 230 °C
3.0 - 8.0 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 53
@Thickness 2.00 mm
53
@Thickness 0.0787 in
ASTM D2240
Tensile Strength at Break 25.0 - 45.0 MPa
@Thickness 2.00 mm
3630 - 6530 psi
@Thickness 0.0787 in
50 mm/min,Type IV; ASTM D638
Tensile Strength, Yield 10.0 - 25.0 MPa
@Thickness 2.00 mm
1450 - 3630 psi
@Thickness 0.0787 in
50 mm/min,Type IV; ASTM D638
Elongation at Break 350 - 600 %
@Thickness 2.00 mm
350 - 600 %
@Thickness 0.0787 in
50 mm/min,Type IV; ASTM D638
Elongation at Yield 10 - 20 %
@Thickness 2.00 mm
10 - 20 %
@Thickness 0.0787 in
50 mm/min,Type IV; ASTM D638
Tensile Modulus 0.450 - 0.650 GPa
@Thickness 2.00 mm
65.3 - 94.3 ksi
@Thickness 0.0787 in
1.0 mm/min, Type IV; ASTM D638
Izod Impact, Notched 10.0 J/cm
@Thickness 4.00 mm
18.7 ft-lb/in
@Thickness 0.157 in
ASTM D256
Coefficient of Friction, Dynamic 0.20 - 0.300.20 - 0.30vs. Itself; ASTM D1894
Coefficient of Friction, Static 0.20 - 0.400.20 - 0.40vs. Itself; ASTM D1894
Taber Abrasion, mg/1000 Cycles 5.0 - 105.0 - 10CS-10 Wheel, 1000 g, 1000 Cycles; ASTM D1044
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cmASTM D257
Surface Resistance >= 1.00e+14 ohm>= 1.00e+14 ohmASTM D257
Dielectric Constant 7.0
@Frequency 1000 Hz
7.0
@Frequency 1000 Hz
ASTM D150
Dielectric Strength 20.0 - 25.0 kV/mm
@Thickness 1.00 mm
508 - 635 kV/in
@Thickness 0.0394 in
ASTM D149
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 23.0 - 29.0 J/g9.89 - 12.5 BTU/lbASTM D3417
CTE, linear, Parallel to Flow 130 - 150 µm/m-°C
@Temperature 0.000 - 40.0 °C
72.2 - 83.3 µin/in-°F
@Temperature 32.0 - 104 °F
ASTM D696
Specific Heat Capacity  1.20 J/g-°C
@Temperature 23.0 °C
0.287 BTU/lb-°F
@Temperature 73.4 °F
ASTM C351
 1.60 J/g-°C
@Temperature 100 °C
0.382 BTU/lb-°F
@Temperature 212 °F
ASTM C351
Thermal Conductivity 0.200 W/m-K1.39 BTU-in/hr-ft²-°FASTM C177
Melting Point 162 - 171 °C324 - 340 °F
Crystallization Temperature 125 - 131 °C257 - 268 °FPeak; ASTM D3418
Vicat Softening Point 110 °C230 °FRate A (50°C/h), Loading 2 (50 N); ASTM D1525
Glass Transition Temp, Tg -28.0 °C-18.4 °FASTM E1356
Flammability, UL94 V-0
@Thickness 0.100 mm
V-0
@Thickness 0.00394 in
Oxygen Index >= 90 %
@Thickness 3.00 mm
>= 90 %
@Thickness 0.118 in
ASTM D2863
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 Latin America
 North America
FormsGranules

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSOL8Y4471 / 280271

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.