MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Akrochem AKROWAXES™ MICRO 23 Bead Wax
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Product Description: AKROWAX Micro 23 is a 100% microcrystalline wax. Microcrystalline refers to the complex mixture of long chain straight paraffins, branched paraffins, as well as mono and polycyclic aliphatic materials. The high molecular weight gives this wax a high melt point; the branching results in a flexible wax film. AKROWAX 23 migrates slowly to the surface of a rubber part. For this reason it should not be used alone for ozone protection. Typically, Micro 23 wax is blended with fast migrating, lower melt point paraffin waxes to provide a bloomed film that has good flexibility and has a wide service temperature range. Akrochem has a wide line of pre-blended waxes to fit most applications. Microcrystalline wax also functions as a good internal release and flow promoter in rubber compounds. This wax complies with F.D.A. Regulations for use as indirect or direct food additives described in Code of Federal Regulations, Title 21, Chapter 1, Section 172.886 and 178.3710 as well as 177.2600, Rubber Articles Intended For Repeated Use.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.930 g/cc
Kinematic Viscosity 20.4 cSt
@Temperature 100 °C
 
Mechanical PropertiesOriginal ValueComments
Penetration 18[dmm], Needle
 
Thermal PropertiesOriginal ValueComments
Dropping Point 186 °FASTM D87
 
Descriptive Properties
AppearanceBead
Color0.5ASTM

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAKZCH634 / 315552

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.