MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Lord Adhesives Chemlok® 205LH Primer
Categories: Polymer

Material Notes: LORD Chemlok® 205LH primer is a low Hazardous Air Pollutant (HAP) primer designed for use under Chemlok covercoat adhesives to bond a wide variety of vulcanized and unvulcanized rubber compounds to metals and other rigid substrates. It is composed of a mixture of polymers, organic compounds and mineral fillers dissolved or dispersed in a low HAP organic solvent system.

Features: can be used as a primer under a variety of Chemlok covercoat adhesives such as the Chemlok 6125 series or Chemlok 6254 series adhesives. applies easily by brush, dip, spray or roll coat methods; suitable for existing production lines. provides rubber tearing bonds and excellent environmental resistance when used in combination with Chemlok covercoat adhesives. provides a brilliant blue color for easy identification when used over phosphatized substrates. contains low HAP content (3.6 lb HAP/gal solid or 6.45% HAP content).

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.40 - 8.00 lb/gal
Solids Content 21.5 - 26.5 %by weight
Brookfield Viscosity 10 - 550 cP
@Temperature 25.0 °C,
Time 10.0 - 100 sec
Brookfield LVT, Spindle 2, 30 rpm, Zahn Cup #2
 
Thermal PropertiesOriginal ValueComments
Flash Point 13.0 °CSeta
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
@Temperature 21.0 - 27.0 °C
from shipment date in original, unopened container
 
Descriptive Properties
AppearanceBlue liquid
SolventsMethyl Propyl Ketone (MPK), N-butyl Propionate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLORD9034 / 232423

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.