MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Lubrizol Advanced Materials Stat-Rite® E1140 TPU/Polyester
Categories: Polymer; Thermoplastic; Polyester, TP

Material Notes: Product Description: E1140 is a static dissipative thermoplastic polyurethane (TPU) alloy, Stat-Rite E1140 utilizes the patented Stat-Rite inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD protection. Stat-Rite alloys retain uniform static dissipation properties even when injection molded or extruded.
Availability: Asia Pacific, Europe, Latin America, North America
Additive: Antistatic
Features: Antistatic; ESD Protection; High Clarity; Low )to None) Ion Content; Low to No Outgassing
Uses: Building Materials; Electrical/Electronic Applications; Tubing
Appearance: Clear/Transparent
Forms: Pellets
Processing Method: Extrusion; Injection Molding

Information provided by Lubrizol Advanced Materials, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 82ASTM D2240
Tensile Strength at Break 4350 psiASTM D412
Tensile Stress 740 psi
@Strain 100 %
ASTM D412
 1160 psi
@Strain 300 %
ASTM D412
Elongation at Break 670 %ASTM D412
Tear Strength 371 pliASTM D624
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.00e+10 ohm-cmASTM D257
Surface Resistance 1.00e+10 ohm12% RH; ESD S11.11
 1.00e+11 ohmASTM D257
Static Decay 0.90 sec5000 V to 50 V, FTMS-101C, 12% RH
 0.90 sec-5000 V to -50 V, FTMS-101C, 12% RH
 
Processing PropertiesOriginal ValueComments
Drying Temperature 221 °F
Dry Time 2.00 - 3.00 hour
 
Descriptive Properties
Ionic Content0.06 mg/m2Anions NO3
 0.2 mg/m2Anions SO4
 0.9 mg/m2Anions Cl
 5 mg/m2Anions PO4
Outgassing<0.1 ppmTotal Organics

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLUBR6013 / 268315

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.